TIG Lasdraad


Tig wire suitable to weld mild and carbon steels; INETIG is generally used in root pass and to support the welding when no back pass is possible. Excellent mechanical and toughness properties when in low temperature conditions.

 

 WELDING PROCESS  
     
 GTAW 

 

 CHEMICAL ANALYSIS  
     
 Mn   1.45 % 
 Si   0.80 % 
 Cu   0.15 % 
 C   0.08 % 
 P   0.012 % 
 S   0.012 % 

 

 DIAMETERS  
     
 1.2 mm (0.045 ")
 1.6 mm (0.062 ")
 2.0 mm (0.078 ")
 2.4 mm (0.094 ")
 3.2 mm (0.125 ")
 4.0 mm (0.156 ")

 

 CLASSIFICATIONS  
     
 AWS A 5.18: ER70S-6 
 EN 1668: W3Si1 

 

 MECHANICAL CHARACTERISTICS WITH Argon   
     
 Elongation   28 %
 Impact test Kv (+20°C)   160 J
 Impact test Kv (-20°C)   120 J
 Impact test Kv (-30°C)   90 J
 Impact test Kv (-40°C)   70 J
 Tensile strength   580 N/mm²
 Yield strength   480 N/mm²

 

 APPROVALS  
     
 DB 
 TUV 

 

 APPLICATIONS  
     
 Carbon steel 
 Carriage-builder 
 Maintenance 
 Pipelines 
 Structural work 

 

 WELDING POSITIONS  
     
 All positions 

 

 PACKING